Rocksolid Light

Welcome to novaBBS (click a section below)

mail  files  register  newsreader  groups  login

Message-ID:  

19 May, 2024: Line wrapping has been changed to be more consistent with Usenet standards.
 If you find that it is broken please let me know here rocksolid.nodes.help


tech / sci.engr.joining.welding / Re: MIG wire speed control problems

SubjectAuthor
* Re: MIG wire speed control problemsThesykboy
`* Re: MIG wire speed control problemsJim Wilkins
 `* Re: MIG wire speed control problemsRichard Smith
  `* Re: MIG wire speed control problemsThesykboy
   `- Re: MIG wire speed control problemsJim Wilkins

1
Re: MIG wire speed control problems

<175ed073079f0ac8$36$565070$c3d349d6@news.newsgroupdirect.com>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=362&group=sci.engr.joining.welding#362

  copy link   Newsgroups: sci.engr.joining.welding
From: f751a351...@example.com (Thesykboy)
Newsgroups: sci.engr.joining.welding
Subject: Re: MIG wire speed control problems
X-Poster: Hermes 2.0
References: <XnS9g.2372$x4.1830@newsread3.news.pas.earthlink.net> <44683734.854167@free.teranews.com> <6ttdg.5329$921.2125@newsread4.news.pas.earthlink.net> <f3dd72155e2op40096mitegn9vpumhmonb@4ax.com> <xbYdg.176$eB3.103@newsread3.news.pas.earthlink.net>
In-Reply-To: <xbYdg.176$eB3.103@newsread3.news.pas.earthlink.net>
Content-Transfer-Encoding: 8bit
Injection-Info: 6b4fc0d3e453ddd24dc657c7b551cb88;e231bac3233fa3c283dbb24936d7f027
Content-Type: text/plain; charset="iso-8859-1"; format="flowed"
Lines: 11
Path: i2pn2.org!i2pn.org!weretis.net!feeder8.news.weretis.net!newsreader4.netcologne.de!news.netcologne.de!peer01.ams1!peer.ams1.xlned.com!news.xlned.com!peer01.iad!feed-me.highwinds-media.com!news.highwinds-media.com!feeder.usenetexpress.com!tr2.iad1.usenetexpress.com!news.newsgroupdirect.com!not-for-mail
Date: Sat, 13 May 2023 21:15:03 +0000
Nntp-Posting-Date: Sat, 13 May 2023 21:15:03 +0000
Organization: NewsgroupDirect
X-Complaints-To: abuse@newsgroupdirect.com
Message-Id: <175ed073079f0ac8$36$565070$c3d349d6@news.newsgroupdirect.com>
X-Received-Bytes: 2529
 by: Thesykboy - Sat, 13 May 2023 21:15 UTC

Hey gang, I read this thread in hopes of finding the cure to my issue (which is similar). Got a Craftsman (Century) from 1992. First time in years I’ve used it and I’ve noticed the wire feed is slow AND weak. I can literally stop the wire feed roller with my fingers (and reasonable pressure) on full speed. I’ve replace the gun, liner, and everything recently because the old one was just too stiff. I also did so in hopes it would solve the feed issue… nope.

I’ve tested the motor on a 12v battery directly and can see that it and the gearbox are working fine - torque and speed. It was hauling ass and I couldn’t stop it with the same pressure as before. I spoke to someone at Lincoln (who now owns Century) and was told the board is likely not putting out the amps the motor needs for proper torque. I just bought the board, but don’t want to throw parts at it. I know something isn’t putting out the right amount of juice and I’m trying to figure out where it’s NOT coming from. Does this make sense to anyone else? I know things get old and stop working, but like the others, I’m not familiar with circuitry and and reluctant to just throw parts at it. I love this welder and really want it to work.

Thanks in advance for the knowledge.

-Jason from Denver.

--
For full context, visit https://www.polytechforum.com/welding/mig-wire-speed-control-problems-9075-.htm

Re: MIG wire speed control problems

<u3p1s4$2bq93$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=363&group=sci.engr.joining.welding#363

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!news.eternal-september.org!.POSTED!not-for-mail
From: muratla...@gmail.com (Jim Wilkins)
Newsgroups: sci.engr.joining.welding
Subject: Re: MIG wire speed control problems
Date: Sat, 13 May 2023 18:09:00 -0400
Organization: A noiseless patient Spider
Lines: 2
Message-ID: <u3p1s4$2bq93$1@dont-email.me>
References: <XnS9g.2372$x4.1830@newsread3.news.pas.earthlink.net> <44683734.854167@free.teranews.com> <6ttdg.5329$921.2125@newsread4.news.pas.earthlink.net> <f3dd72155e2op40096mitegn9vpumhmonb@4ax.com> <xbYdg.176$eB3.103@newsread3.news.pas.earthlink.net> <175ed073079f0ac8$36$565070$c3d349d6@news.newsgroupdirect.com>
MIME-Version: 1.0
Content-Type: text/plain;
format=flowed;
charset="UTF-8";
reply-type=response
Content-Transfer-Encoding: 8bit
Injection-Date: Sat, 13 May 2023 22:10:12 -0000 (UTC)
Injection-Info: dont-email.me; posting-host="47e1980a20f4fdea65794b2f833b112e";
logging-data="2484515"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX19fXxjvKn9Qbt7gtIR1WMvZlrNmTNOCsrI="
Cancel-Lock: sha1:tEAzXe6Wgg9vQv2lAnZvhNpU2BM=
X-MimeOLE: Produced By Microsoft MimeOLE V16.4.3505.912
X-MSMail-Priority: Normal
Importance: Normal
X-Antivirus: AVG (VPS 230513-4, 5/13/2023), Outbound message
X-Antivirus-Status: Clean
In-Reply-To: <175ed073079f0ac8$36$565070$c3d349d6@news.newsgroupdirect.com>
X-Priority: 3
X-Newsreader: Microsoft Windows Live Mail 16.4.3505.912
 by: Jim Wilkins - Sat, 13 May 2023 22:09 UTC

"Thesykboy" wrote in message
news:175ed073079f0ac8$36$565070$c3d349d6@news.newsgroupdirect.com...

Hey gang, I read this thread in hopes of finding the cure to my issue
(which is similar). Got a Craftsman (Century) from 1992. First time in years
I’ve used it and I’ve noticed the wire feed is slow AND weak. I can
literally stop the wire feed roller with my fingers (and reasonable
pressure) on full speed. I’ve replace the gun, liner, and everything
recently because the old one was just too stiff. I also did so in hopes it
would solve the feed issue… nope.

I’ve tested the motor on a 12v battery directly and can see that it and
the gearbox are working fine - torque and speed. It was hauling ass and I
couldn’t stop it with the same pressure as before. I spoke to someone at
Lincoln (who now owns Century) and was told the board is likely not putting
out the amps the motor needs for proper torque. I just bought the board, but
don’t want to throw parts at it. I know something isn’t putting out the
right amount of juice and I’m trying to figure out where it’s NOT coming
from. Does this make sense to anyone else? I know things get old and stop
working, but like the others, I’m not familiar with circuitry and and
reluctant to just throw parts at it. I love this welder and really want it
to work.

Thanks in advance for the knowledge.

-Jason from Denver.

---------------------

Posted to sci.engr.joining.welding

The schematic for a Century Powermate 70 shows two apparently selenium
rectifiers, a speed control pot and the torch switch in the wire feed motor
drive. Any of them could be the problem.
-jsw

Re: MIG wire speed control problems

<ly8rdq4rk9.fsf@void.com>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=364&group=sci.engr.joining.welding#364

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!weretis.net!feeder6.news.weretis.net!newsfeed.hasname.com!usenet.blueworldhosting.com!diablo1.usenet.blueworldhosting.com!nnrp.usenet.blueworldhosting.com!.POSTED!not-for-mail
From: nul...@void.com (Richard Smith)
Newsgroups: sci.engr.joining.welding
Subject: Re: MIG wire speed control problems
Date: Sun, 14 May 2023 20:54:30 +0100
Organization: BlueWorld Hosting Usenet (https://usenet.blueworldhosting.com)
Message-ID: <ly8rdq4rk9.fsf@void.com>
References: <XnS9g.2372$x4.1830@newsread3.news.pas.earthlink.net> <44683734.854167@free.teranews.com> <6ttdg.5329$921.2125@newsread4.news.pas.earthlink.net> <f3dd72155e2op40096mitegn9vpumhmonb@4ax.com> <xbYdg.176$eB3.103@newsread3.news.pas.earthlink.net> <175ed073079f0ac8$36$565070$c3d349d6@news.newsgroupdirect.com> <u3p1s4$2bq93$1@dont-email.me>
MIME-Version: 1.0
Content-Type: text/plain; charset=utf-8
Content-Transfer-Encoding: 8bit
Injection-Info: nnrp.usenet.blueworldhosting.com;
logging-data="84547"; mail-complaints-to="usenet@blueworldhosting.com"
User-Agent: Gnus/5.11 (Gnus v5.11) Emacs/22.1 (darwin)
Cancel-Lock: sha1:bAi+oiWOrGOvFiHewhZ0p1Gl7no=
sha1:GTDAMWI6q7q9V56eRt3M9hxorPM= sha256:IN+HJg5GDINvxflh17xOAAvriK51pXc0KirmmNVc7fc=
sha1:pw3tTk4AnBRBnqk0m1N7qlhToZ4= sha256:Yul8VdPoy7h6lrd7eQBREr6nObe1oFl4FuOcMy65ozQ=
 by: Richard Smith - Sun, 14 May 2023 19:54 UTC

"Jim Wilkins" <muratlanne@gmail.com> writes:

> "Thesykboy" wrote in message
> news:175ed073079f0ac8$36$565070$c3d349d6@news.newsgroupdirect.com...
>
> Hey gang, I read this thread in hopes of finding the cure to my issue
> (which is similar). Got a Craftsman (Century) from 1992. First time in
> years I’ve used it and I’ve noticed the wire feed is slow AND
> weak. I can literally stop the wire feed roller with my fingers (and
> reasonable pressure) on full speed. I’ve replace the gun, liner, and
> everything recently because the old one was just too stiff. I also did
> so in hopes it would solve the feed issue… nope.
>
> I’ve tested the motor on a 12v battery directly and can see that it
> and the gearbox are working fine - torque and speed. It was hauling
> ass and I couldn’t stop it with the same pressure as before. I spoke
> to someone at Lincoln (who now owns Century) and was told the board is
> likely not putting out the amps the motor needs for proper torque. I
> just bought the board, but don’t want to throw parts at it. I know
> something isn’t putting out the right amount of juice and I’m
> trying to figure out where it’s NOT coming from. Does this make
> sense to anyone else? I know things get old and stop working, but like
> the others, I’m not familiar with circuitry and and reluctant to
> just throw parts at it. I love this welder and really want it to work.
>
> Thanks in advance for the knowledge.
>
> -Jason from Denver.
>
> ---------------------
>
> Posted to sci.engr.joining.welding
>
> The schematic for a Century Powermate 70 shows two apparently selenium
> rectifiers, a speed control pot and the torch switch in the wire feed
> motor drive. Any of them could be the problem.
> -jsw

A wider overall point:

With a MIG / GMAW welder, you deliberately set the drive rolls so they
will skid if the wire jams.
You set the pressure so the wire will feed, but any more resistance
than regular feed and the rolls slip on the wire.
That's the reason for the springs on the toggles mechanism for the
drive rolls.

Re: MIG wire speed control problems

<175f24e35dcf3418$1$3685597$13d399db@news.newsgroupdirect.com>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=365&group=sci.engr.joining.welding#365

  copy link   Newsgroups: sci.engr.joining.welding
From: f751a351...@example.com (Thesykboy)
Newsgroups: sci.engr.joining.welding
Subject: Re: MIG wire speed control problems
X-Poster: Hermes 2.0
References: <XnS9g.2372$x4.1830@newsread3.news.pas.earthlink.net> <44683734.854167@free.teranews.com> <6ttdg.5329$921.2125@newsread4.news.pas.earthlink.net> <f3dd72155e2op40096mitegn9vpumhmonb@4ax.com> <xbYdg.176$eB3.103@newsread3.news.pas.earthlink.net> <175ed073079f0ac8$36$565070$c3d349d6@news.newsgroupdirect.com> <u3p1s4$2bq93$1@dont-email.me> <ly8rdq4rk9.fsf@void.com>
In-Reply-To: <ly8rdq4rk9.fsf@void.com>
Content-Transfer-Encoding: 8bit
Injection-Info: 6b4fc0d3e453ddd24dc657c7b551cb88;5f6b0c81d77164010a5bfeefae54e21e
Content-Type: text/plain; charset="iso-8859-1"; format="flowed"
Lines: 9
Path: i2pn2.org!i2pn.org!newsfeed.endofthelinebbs.com!usenet.blueworldhosting.com!diablo1.usenet.blueworldhosting.com!peer02.iad!feed-me.highwinds-media.com!news.highwinds-media.com!feeder.usenetexpress.com!tr2.iad1.usenetexpress.com!news.newsgroupdirect.com!not-for-mail
Date: Sun, 14 May 2023 23:02:24 +0000
Nntp-Posting-Date: Sun, 14 May 2023 23:02:24 +0000
Organization: NewsgroupDirect
X-Complaints-To: abuse@newsgroupdirect.com
Message-Id: <175f24e35dcf3418$1$3685597$13d399db@news.newsgroupdirect.com>
X-Received-Bytes: 2235
 by: Thesykboy - Sun, 14 May 2023 23:02 UTC

The problem is, there doesn’t seem to be enough amps to the feed motor to power it with the torque it needs to move the wire. I’ve run the wire through 2 different liners and the resistance in the feed is the same. So I’m guessing the motor has to have a bit of torque to feed the wire.

Last night I tested amps where the leads come from the board to the motor. When the pot is set at 2, it reads .26 amps. When I keep cranking it up to 6, it hits .30 amps, and at 8…. same .30 amps. I’ve looked at other motors online to get a baseline of how many amps that motor should need to do its job. Even the cheap ones on Amazon are doing .90, so I’m thinking the amps coming from the board are way too low. I found a company that sells a new OE board with pot and voltage dials on it for a decent price. I don’t want to just throw parts at it, but in my research so far, everything points to what is sending amps the the motor… the board.

Sound about right?

--
For full context, visit https://www.polytechforum.com/welding/mig-wire-speed-control-problems-9075-.htm

Re: MIG wire speed control problems

<u3rqr3$2orru$1@dont-email.me>

  copy mid

https://www.novabbs.com/tech/article-flat.php?id=366&group=sci.engr.joining.welding#366

  copy link   Newsgroups: sci.engr.joining.welding
Path: i2pn2.org!i2pn.org!eternal-september.org!news.eternal-september.org!.POSTED!not-for-mail
From: muratla...@gmail.com (Jim Wilkins)
Newsgroups: sci.engr.joining.welding
Subject: Re: MIG wire speed control problems
Date: Sun, 14 May 2023 19:27:24 -0400
Organization: A noiseless patient Spider
Lines: 1
Message-ID: <u3rqr3$2orru$1@dont-email.me>
References: <XnS9g.2372$x4.1830@newsread3.news.pas.earthlink.net> <44683734.854167@free.teranews.com> <6ttdg.5329$921.2125@newsread4.news.pas.earthlink.net> <f3dd72155e2op40096mitegn9vpumhmonb@4ax.com> <xbYdg.176$eB3.103@newsread3.news.pas.earthlink.net> <175ed073079f0ac8$36$565070$c3d349d6@news.newsgroupdirect.com> <u3p1s4$2bq93$1@dont-email.me> <ly8rdq4rk9.fsf@void.com> <175f24e35dcf3418$1$3685597$13d399db@news.newsgroupdirect.com>
MIME-Version: 1.0
Content-Type: text/plain;
format=flowed;
charset="UTF-8";
reply-type=response
Content-Transfer-Encoding: 8bit
Injection-Date: Sun, 14 May 2023 23:28:35 -0000 (UTC)
Injection-Info: dont-email.me; posting-host="1fb4c6e62e2868a1a11b3017c712e45d";
logging-data="2912126"; mail-complaints-to="abuse@eternal-september.org"; posting-account="U2FsdGVkX1/X23OjrbCvev+dwzpxoIlETCk6U+V7J1Q="
Cancel-Lock: sha1:dwHq94sIsFHNraNJz/s3jqgmJyM=
Importance: Normal
X-Priority: 3
X-Antivirus-Status: Clean
In-Reply-To: <175f24e35dcf3418$1$3685597$13d399db@news.newsgroupdirect.com>
X-MSMail-Priority: Normal
X-Antivirus: AVG (VPS 230514-4, 5/14/2023), Outbound message
X-Newsreader: Microsoft Windows Live Mail 16.4.3505.912
X-MimeOLE: Produced By Microsoft MimeOLE V16.4.3505.912
 by: Jim Wilkins - Sun, 14 May 2023 23:27 UTC

"Thesykboy" wrote in message
news:175f24e35dcf3418$1$3685597$13d399db@news.newsgroupdirect.com...

The problem is, there doesn’t seem to be enough amps to the feed motor to
power it with the torque it needs to move the wire. I’ve run the wire
through 2 different liners and the resistance in the feed is the same. So
I’m guessing the motor has to have a bit of torque to feed the wire.

Last night I tested amps where the leads come from the board to the motor.
When the pot is set at 2, it reads .26 amps. When I keep cranking it up to
6, it hits .30 amps, and at 8…. same .30 amps. I’ve looked at other
motors online to get a baseline of how many amps that motor should need to
do its job. Even the cheap ones on Amazon are doing .90, so I’m thinking
the amps coming from the board are way too low. I found a company that sells
a new OE board with pot and voltage dials on it for a decent price. I
don’t want to just throw parts at it, but in my research so far,
everything points to what is sending amps the the motor… the board.

Sound about right?

------------------------------

A partly open bridge rectifier diode will give you the no-load voltage but
not the full current. Half-wave rectification is obvious if you have an
oscilloscope. It might show up as a large voltage difference between when
the motor is connected and disconnected.

If you can find an electrical schematic for it I might be able to suggest
other tests to locate the fault.


tech / sci.engr.joining.welding / Re: MIG wire speed control problems

1
server_pubkey.txt

rocksolid light 0.9.81
clearnet tor